I-Nimonic 80A/UNS N07080
Ingxubevange | isiqalelo | C | Si | Mn | S | Ni | Cr | Al | Ti | Fe | Cu | Co | B |
UNimonic80A | Min | 18.0 | 1.0 | 1.8 | |||||||||
Max | 0.1 | 1.0 | 1.0 | 0.015 | Ibhalansi | 21.0 | 1.8 | 2.7 | 3.0 | 0.2 | 2.0 | 0.008 | |
Oapho | Zr:0.15Ubukhulu,Pb:0.0025Ubukhulu, |
AuloyiUbume | Tensile strength Rm Mpa min. | Unikeze Amandla RP 0. 2Mpa min. | Ukwandisa A 5 % |
Suhlengahlengiso &imvula | 1000 | 620 | 2 |
Ukuxinanag/cm3 | Indawo yokunyibilika℃ |
8.19 | 1320~1365 |
Intonga, iBar, ucingo kunye ne-Forging Stock- BS 3076 & HR 1; I-ASTM B 637
Ipleyiti, iPhepha kunye nomtya -I-BS HR 201
Umbhobho kunye netyhubhu-BS HR 401
Bhala umyalezo wakho apha kwaye uwuthumele kuthi