Kovar/UNS K94610
Ingxubevange | isiqalelo | C | Si | Mn | S | P | Ni | Fe | Co | Mo |
Kovar | Min |
|
|
|
|
| 28.5 |
| 16.8 |
|
Max | 0.03 | 0.3 | 0.5 | 0.02 | 0.02 | 29.5 | ibhalansi | 17.8 | 0.2 |
Isimo se-Aolly | I-Linear Coefficient(10-6/°C) | ||||
20-200℃ | 20-300℃ | 20-400℃ | 20~500℃ | 20-600℃ | |
isusiwe | 5.9 | 5.3 | 5.1 | 6.2 | 7.8 |
Ukuxinanag/cm3 | Indawo yokunyibilika℃ |
8.16 | 1450 |
Intonga, iBar, ucingo kunye ne-Forging Stock-ASTM F15
Ipleyiti, iPhepha kunye nomtya -SAE AMS 7728
Bhala umyalezo wakho apha kwaye uwuthumele kuthi